AFM Tips at the Very End of the AFM Cantilever

AFM probes with 3-sided pyramidal macroscopic shape of the AFM tips for optimized positioning upon sample (OPUS)
Sort by:
32 results
top value
3XC-NA
3XC-NA

AFM Probe with 3 Different AFM Cantilevers for Various Applications and AFM  Tips at the Very End of the AFM Cantilevers

Coating: Reflective Aluminum
Tip Shape: Optimized Positioning
AFM Cantilevers: 3
1
2
3
F
17 kHz
150 kHz
75 kHz
C
0.3 N/m
9 N/m
2.5 N/m
L
500 µm
175 µm
240 µm
160AC-NN
160AC-NN
Standard Tapping Mode AFM Probe with AFM Tip at the Very End of the AFM Cantilever
Coating: none
Tip Shape: Optimized Positioning
AFM Cantilever:
F
300 kHz
C
26 N/m
L
160 µm
240AC-NN
240AC-NN
Force Modulation AFM Probe with AFM Tip at the Very End of the AFM Cantilever
Coating: none
Tip Shape: Optimized Positioning
AFM Cantilever:
F
70 kHz
C
2 N/m
L
240 µm
3XC-NN
3XC-NN
AFM Probe with 3 Different AFM Cantilevers for Various Applications and AFM  Tips at the Very End of the AFM Cantilevers
Coating: none
Tip Shape: Optimized Positioning
AFM Cantilevers: 3
1
2
3
F
17 kHz
150 kHz
75 kHz
C
0.3 N/m
9 N/m
2.5 N/m
L
500 µm
175 µm
240 µm
4XC-NN
4XC-NN
AFM Probe with 4 Different AFM Cantilevers with AFM Tips at the Very End of the AFM Cantilevers
Coating: none
Tip Shape: Optimized Positioning
AFM Cantilevers: 4
1
2
3
4
F
17 kHz
75 kHz
150 kHz
1200 kHz
C
0.3 N/m
2.5 N/m
9 N/m
100 N/m
L
500 µm
240 µm
175 µm
65 µm
top value
160AC-FG
160AC-FG
High Aspect Ratio, Tapping Mode AFM Probe with AFM Tip at the Very End of the AFM Cantilever
Coating: Reflective Gold
Tip Shape: High-Aspect-Ratio
AFM Cantilever:
F
300 kHz
C
26 N/m
L
160 µm
New
240AC-FG
240AC-FG
High Aspect Ratio, Force Modulation AFM Probe with AFM Tip at the Very End of the AFM Cantilever
Coating: Reflective Gold
Tip Shape: High-Aspect-Ratio
AFM Cantilever:
F
70 kHz
C
2 N/m
L
240 µm
3XC-GG
3XC-GG
AFM Probe with 3 Different Gold Coated AFM Cantilevers for Various Applications and AFM Tips at the Very End of the AFM Cantilevers
Coating: Gold Overall
Tip Shape: Optimized Positioning
AFM Cantilevers: 3
1
2
3
F
17 kHz
150 kHz
75 kHz
C
0.3 N/m
9 N/m
2.5 N/m
L
500 µm
175 µm
240 µm
4XC-GG
4XC-GG
AFM Probe with 4 Different Gold Coated AFM Cantilevers with AFM Tips at the Very End of the AFM Cantilevers
Coating: Gold Overall
Tip Shape: Optimized Positioning
AFM Cantilevers: 4
1
2
3
4
F
17 kHz
75 kHz
150 kHz
1200 kHz
C
0.3 N/m
2.5 N/m
9 N/m
100 N/m
L
500 µm
240 µm
175 µm
65 µm
240AC-GG
240AC-GG
Gold Coated Force Modulation AFM Probe with AFM Tip at the Very End of the AFM Cantilever
Coating: Gold Overall
Tip Shape: Optimized Positioning
AFM Cantilever:
F
70 kHz
C
2 N/m
L
240 µm
160AC-GG
160AC-GG
Gold Coated Tapping Mode AFM Probe with AFM Tip at the Very End of the AFM Cantilever
Coating: Gold Overall
Tip Shape: Optimized Positioning
AFM Cantilever:
F
300 kHz
C
26 N/m
L
160 µm
New
BL-AC40TS
BL-AC40TS
Tapping Mode AFM Probe for High-Speed Scanning in Liquids
Coating: Reflective Gold
Tip Shape: Optimized Positioning
AFM Cantilever:
F
110 kHz
C
0.1 N/m
L
38 µm
2