Tap300GB-G
Tap300GB-G
Gold Coated Tapping Mode AFM Probe
Coating: Gold Overall
Tip Shape: Rotated
AFM Cantilever:
F
300 kHz
C
40 N/m
L
125 µm
Tap190GB-G
Tap190GB-G
Gold Coated Tapping Mode AFM Probe with Long AFM Cantilever
Coating: Gold Overall
Tip Shape: Rotated
AFM Cantilever:
F
190 kHz
C
48 N/m
L
225 µm
160AC-GG
160AC-GG
Gold Coated Tapping Mode AFM Probe with AFM Tip at the Very End of the AFM Cantilever
Coating: Gold Overall
Tip Shape: Optimized Positioning
AFM Cantilever:
F
300 kHz
C
26 N/m
L
160 µm
HQ:NSC14/Cr-Au
HQ:NSC14/Cr-Au
Gold Coated Soft Tapping Mode AFM Probe
Coating: Gold Overall
Tip Shape: Rotated
AFM Cantilever:
F
160 kHz
C
5 N/m
L
125 µm
HQ:NSC15/Cr-Au
HQ:NSC15/Cr-Au
Gold Coated Tapping Mode AFM Probe
Coating: Gold Overall
Tip Shape: Rotated
AFM Cantilever:
F
325 kHz
C
40 N/m
L
125 µm
HQ:NSC16/Cr-Au
HQ:NSC16/Cr-Au
Gold Coated Tapping Mode AFM Probe with Long AFM Cantilever
Coating: Gold Overall
Tip Shape: Rotated
AFM Cantilever:
F
190 kHz
C
45 N/m
L
225 µm
Tap150GB-G
Tap150GB-G
Gold Coated Soft Tapping Mode AFM Probe
Coating: Gold Overall
Tip Shape: Rotated
AFM Cantilever:
F
150 kHz
C
5 N/m
L
125 µm
SSS-QMFMR
SSS-QMFMR
SuperSharp, Hard Magnetic, Low Momentum MFM AFM Probe with a High Mechanical Q-Factor
Coating: Magnetic
Tip Shape: Supersharp
AFM Cantilever:
F
75 kHz
C
2.8 N/m
L
225 µm
PPP-LM-MFMR
PPP-LM-MFMR
Hard Magnetic, Low Momentum MFM AFM Probe
Coating: Magnetic
Tip Shape: Standard
AFM Cantilever:
F
75 kHz
C
2.8 N/m
L
225 µm
PPP-LC-MFMR
PPP-LC-MFMR
Soft Magnetic, Medium Momentum MFM AFM Probe
Coating: Magnetic
Tip Shape: Standard
AFM Cantilever:
F
75 kHz
C
2.8 N/m
L
225 µm
PPP-QLC-MFMR
PPP-QLC-MFMR
Soft Magnetic, Medium Momentum MFM AFM Probe with a High Mechanical Q-Factor
Coating: Magnetic
Tip Shape: Standard
AFM Cantilever:
F
75 kHz
C
2.8 N/m
L
225 µm
best of the best
TL-CONT
TL-CONT
Tipless Contact Mode AFM Cantilever
Coating: none
Tip Shape: Tipless
AFM Cantilever:
F
13 kHz
C
0.2 N/m
L
450 µm
TL-FM
TL-FM
Tipless Force Modulation AFM Cantilever
Coating: none
Tip Shape: Tipless
AFM Cantilever:
F
75 kHz
C
2.8 N/m
L
225 µm
TL-NCH
TL-NCH
Tipless Tapping Mode AFM Cantilever
Coating: none
Tip Shape: Tipless
AFM Cantilever:
F
330 kHz
C
42 N/m
L
125 µm
TL-NCL
TL-NCL
Tipless, Long Tapping Mode AFM Cantilever
Coating: none
Tip Shape: Tipless
AFM Cantilever:
F
190 kHz
C
48 N/m
L
225 µm
SuperSharpStandard-FM
SuperSharpStandard-FM
SuperSharp diamond-like EBD AFM whisker for soft tapping AFM
Coating: Reflective Aluminum
Tip Shape: Cone Shaped,Supersharp,EBD
AFM Cantilever:
F
75 kHz
C
2.8 N/m
L
225 µm
PPP-ZEIHR
PPP-ZEIHR
Special Tapping Mode AFM Probe
Coating: Reflective Aluminum
Tip Shape: Standard
AFM Cantilever:
F
130 kHz
C
27 N/m
L
225 µm
ZEIHR
ZEIHR
Special Tapping Mode AFM Probe
Coating: Reflective Aluminum
Tip Shape: Standard
AFM Cantilever:
F
130 kHz
C
27 N/m
L
225 µm
PPP-SEIH
PPP-SEIH
Special Tapping Mode AFM Probe
Coating: none
Tip Shape: Standard
AFM Cantilever:
F
130 kHz
C
15 N/m
L
225 µm
PPP-SEIHR
PPP-SEIHR
Special Tapping Mode AFM Probe
Coating: Reflective Aluminum
Tip Shape: Standard
AFM Cantilever:
F
130 kHz
C
15 N/m
L
225 µm
15